Product description ·ER20A-02 is a high performance material,it has excellent scratch risistant effect,can be taken shape rapidly。    Key characteristic 1. It is very bright on the surface 2.very high bonding strength, adhesive material: PP 3.rapid molding,non-stick mold 4. scratch resistance on the surface,not easy to fluff Function   main application Sports equipment   Instrument shell Electronic plastic accessories Processing method Injection molding Environmental certification ROHS REACH EN71-3 PAHS ASTM-F963 Phthalate Color Natural Smell A little resin smell Appearance Cylindrical particle,about 3mm×1.5mm Storage period Ventilated dry at normal temperature,about 24 months Packaging method 25kg/bag Physical properties Result Unit Method Molding condition Specific gravity 1.08±0.02 g/cm3 ASTM D792 Drying temp       70℃ Hardness 22±5 shoreA ASTM D2240 Drying time     2Hours Tensile strength >1 Mpa ASTM D412 Nozzle temp      190℃ Elongation at break >400 % ASTM D412 Screw 1 temp 180℃ Tearing strength >5 Kn/m ASTM D624 Screw 2 temp 170℃ Melt index >40 g/10min ASTM D1238 Screw 3 temp 160℃ Matters need attention Purge compound Please make sure you that you have cleaned the machine screw with PP or PE, and put the machine nozzle thoroughly clean Coloring     Please select color master batch on PE or EVA material with the exception of PVC.Higher screw speed and backpressure and needed for better colorant dispersion Recycling It is recommended that the recovery rate of the secondary material (nozzle material) be at most 20%.  
  • Product Description
  • Product description

    ·ER20A-02 is a high performance material,it has excellent scratch risistant effect,can be taken shape rapidly。   

    Key characteristic

    1. It is very bright on the surface

    2.very high bonding strength, adhesive material: PP

    3.rapid molding,non-stick mold

    4. scratch resistance on the surface,not easy to fluff

    Function

     

    main application

    Sports equipment

     

    Instrument shell

    Electronic plastic accessories

    Processing method

    Injection molding

    Environmental certification

    ROHS

    REACH

    EN71-3

    PAHS

    ASTM-F963

    Phthalate

    Color

    Natural

    Smell

    A little resin smell

    Appearance

    Cylindrical particle,about 3mm×1.5mm

    Storage period

    Ventilated dry at normal temperature,about 24 months

    Packaging method

    25kg/bag

    Physical properties

    Result

    Unit

    Method

    Molding condition

    Specific gravity

    1.08±0.02

    g/cm3

    ASTM D792

    Drying temp       70

    Hardness

    22±5

    shoreA

    ASTM D2240

    Drying time     2Hours

    Tensile strength

    >1

    Mpa

    ASTM D412

    Nozzle temp      190

    Elongation at break

    >400

    %

    ASTM D412

    Screw 1 temp 180

    Tearing strength

    >5

    Kn/m

    ASTM D624

    Screw 2 temp 170

    Melt index

    >40

    g/10min

    ASTM D1238

    Screw 3 temp 160

    Matters need attention

    Purge compound

    Please make sure you that you have cleaned the machine screw with PP or PE, and put the machine nozzle thoroughly clean

    Coloring

     

     

    Please select color master batch on PE or EVA material with the exception of PVC.Higher screw speed and backpressure and needed for better colorant dispersion

    Recycling

    It is recommended that the recovery rate of the secondary material (nozzle material) be at most 20%.

     