The problem of TPE/TPR injection temperature

  Influencing factors: oil filling rate; SEBS/SBS molecular weight and molecular conformation (linear or star); product thickness; special material formulation and equipment and mold problems, etc.

  1. The higher the oil filling ratio, the lower the corresponding injection temperature.

  2. The injection temperature of SEBS base material is higher than that of SBS base material because the thermal stability of SEBS base material is better than that of SBS base material.

  3. SEBS, SBS molecular weight, high injection temperature; star SEBS / SBS system, injection temperature is higher than the linear SEBS / SBS system.

  4. For special materials, such as TPE with sticky PA, the introduction of high melting point phase components in the formulation makes the injection temperature higher.

  5. the injection temperature required for products with large thickness is higher than that for products with thin thickness.

  6. Equipment type or melt capacity, as well as mold design (including runner, inlet design and the number of cavities in a mold, etc.) will have an impact.

  In terms of hardness and injection method, the recommended injection temperature range is as follows (the specific temperature is adjusted according to the TPE grade provided by the supplier combined with the actual processing situation).

  1.TPE hardness 0C~15A super soft material, injection molding temperature 130~200℃;

  2.TPE/TPR hardness 20~110A single material injection material, recommended injection temperature 140~230℃.

  3. TPE/TPR covered PP, the recommended secondary injection temperature 170~200℃;

  4. TPE/TPR encapsulated ABS,PC, the recommended secondary injection temperature is 180~220℃.

  5. TPE/TPR coated PA, the recommended secondary injection temperature is 240~270℃.

  6. TPE/TPR coated PS (HIPS, GPPS), the recommended secondary injection temperature is 160~190℃.

  In short, about TPE/TPR material injection temperature, the general supplier can only give a reference value according to the material type. It should also be combined with the product structure size, processing equipment and mold design and other factors to consider, and gradually adjust the most suitable injection molding temperature according to the actual processing conditions.

  TPE/TPR shrinkage rate, 1 ~ 3%, low hardness TPE shrinkage rate is larger, other formula system is the same, the filling amount of TPE shrinkage rate is smaller than the filling amount of small TPE/TPR.

Related News

塑伯TPE
塑伯橡塑胶
智能穿戴硬件联盟

Copyright © 2021          Guangdong  SPP New Material Co.,LTD

All Rights Reserved       粤ICP备2020127300号

 

TEL:+86-0752-6768128    FAX:+86-0752-6768088     MAIL:sales@tpe-sp.com   WEB:Een.tpe-sp.com

ADD:Huangxi Industrial Park, Shiwan Town, Boluo County, Huizhou City, Guangdong Province,China